MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pyrotek Vacuum Formed Shapes for Continuous Sheet Casting
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Vacuum formed shapes are manufactured from high purity alumina silica fibers in one-piece design that eliminates metal leakage. No pre-heating required. Reusable, with proper treatment, for multiple casting campaigns.

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.514 g/cc0.0186 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.00183 GPa0.265 ksi
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.160 W/m-K
@Temperature 540 °C
1.11 BTU-in/hr-ft²-°F
@Temperature 1000 °F
 0.240 W/m-K
@Temperature 815 °C
1.67 BTU-in/hr-ft²-°F
@Temperature 1500 °F
Maximum Service Temperature, Air 1090 °C1990 °FContinuous
 1260 °C2300 °F
Shrinkage  0.33 %
@Temperature 400 °C
0.33 %
@Temperature 752 °F
 0.33 %
@Temperature 730 °C
0.33 %
@Temperature 1350 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay VTS 243FR Epoxy Syntactic-Core Film
Rogers Arlon Thermavac® 0.020" (0.508 mm) Uncured Silicone Vacuum Bagging (30400R020)
Pyrotek Pyrite Vacuum Formed Product
Petroquimica Triunfo Tritheva® TN 2020 EVA Copolymer
Morgan Advanced Ceramics Inorganic RCF Vacuum Formed Products I-2100 Thermal Ceramic

CPYRO197 / 1914

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.