MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Rogers Arlon Thermavac® 0.020" (0.508 mm) Uncured Silicone Vacuum Bagging (30400R020)
Categories: Polymer; Thermoset; Silicone

Material Notes: Uncured, unsupported silicone rubber with a thickness of 0.020 in ± 0.002 (0.51 mm ± 0.051) on a Kodacel carrier (0.005 in., 0.13 mm nominal thickness); 0.003 in. (0.08 mm) polyethylene interleave. The shelf life is defined as the duration of time for which the product will meet the physical requirements outlined below. It does not guarantee the product’s usefulness in all applications. Color: Red. Weight: 688.3 g/m² ± 67.8 (20.3 oz./yd.² ± 2.0). Shelf Life: 3 months from date of manufacture at 4.4°C (40°F). Cure Time: 0.5 hours. Post Cure: 204°C (400°F), for 4 hours.

Applications: Composite vacuum bagging materials.

Information provided by the manufacturer, Arlon Silicone Technologies Division.

Information provided by Arlon Silicone Technologies; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 50 - 6050 - 60
Tensile Strength, Ultimate 6.21 - 7.59 MPa901 - 1100 psi
Elongation at Break 450 - 550 %450 - 550 %
Tear Strength >= 35.1 kN/m>= 200 pli
Compression Set 28 %28 %after post cure
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength >= 15.75 kV/mm>= 400.0 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 232 °C450 °F
Minimum Service Temperature, Air -56.6 °C-69.9 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 176.6 °C349.9 °Fcuring temp., at 0.345 MPa (50 psi)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pyrotek Vacuum Formed Shapes for Continuous Sheet Casting
Pyrotek Pyrite Vacuum Formed Product
Petroquimica Triunfo Tritheva® TN 2020 EVA Copolymer
NeXolve Thermalbright® C Polyimide Film
Morgan Advanced Ceramics Inorganic RCF Vacuum Formed Products I-2100 Thermal Ceramic

PASF30 / 24749

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.