MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CIMBAR BARIMITE™ UF High Purity Barite (BaSO4)
Categories: Ceramic; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Barimite Products are natural, off-white barites produced in Cartersville, Georgia. Cimbar's broad range of Barimite products are clean, high purity, high specific gravity, low solubility and chemically inert. These properties have made Barimite products the industry standard for consistent quality and performance in a wide range of end-use applications.

Uses:

  • Coatings: Automotive Primers, Automotive Topcoats, High Gloss Enamel, Powder Coatings, Semi-gloss Latexes, Gloss Latexes, Industrial Coatings, Architectural Coatings
  • Fillers: Plastics, Ceramics, Friction Materials, Rubber, Plastisols, Adhesives, Latex Products, Urethane Foams, Acoustical Compounds, Insulating Materials, Sound Attenuation Products

Information provided by Cimbar Performance Minerals.

Key Words: BaSO4, Baryte, Barium Sulfate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 4.39 g/cc
Oil Absorption 13 %
Fineness 7.0Hegman Fineness
Apparent Bulk Density 0.0347 lb/in³Loose
 0.0579 lb/in³Compacted
Moisture Absorption at Equilibrium 0.10 %
Loss On Ignition 0.30 %
Particle Size 1.8 µmMedian
 <= 10 µmMax
Particle Mesh Size 325 Mesh0.0% retained
pH 8.0
 
Component Elements PropertiesOriginal ValueComments
Al2O3 0.060 %
Fe2O3 0.20 %
SiO2 0.50 %
Trace Metals 0.040 %Heavy Metals
 
Descriptive Properties
BaSO4 (%)96

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CIMBAR BARIMITE™ 200 High Purity Barite (BaSO4)
CIMBAR BariScan Elite Chemically Purified White Barium Sulfate (BaSO4)
CIMBAR BARIMITE™ G-50 High Purity Barite (BaSO4)
CIMBAR BARIMITE™ XF High Purity Barite (BaSO4)
CIMBAR CIMBAR™ PC Barite Powder (BaSO4)

CIMBAR908 / 133390

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.