MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CIMBAR BariScan Elite Chemically Purified White Barium Sulfate (BaSO4)
Categories: Ceramic; Other Engineering Material; Additive/Filler for Polymer

Material Notes: BariScan barite products are produced using a proprietary chemical process to enhance the purity of the natural barium sulfate ore. BariScan Elite and BariScan Ultra barite meet and exceed the requirements for barium sulfate of the United States Pharmacopeia (USP) and European Pharmacopeia (EP). Barium Sulfate is Affirmed GRAS (Generally Recognized As Safe) by the US FDA (21 CFR 175.105, 175.300, 175.380, 175.390, 176.170, 177.1210, 177.1350, 177.1460, 177.2600, 182.99. BariScan barite is manufactured in Chatsworth, GA under stringent quality assurance procedures and Good manufacturing Practices (GMP). The Chatsworth Pharmaceutical Plant is registered with the US FDA as an Active Pharmaceutical Ingredients manufacturer.

Information provided by Cimbar Performance Minerals.

Key Words: BaSO4, Baryte, Barium Sulfate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 4.40 g/cc4.40 g/cc
Fineness 7.07.0Hegman Fineness
Loss On Ignition <= 2.0 %<= 2.0 %
Particle Size 1.0 µm1.0 µmMedian
 <= 12 µm<= 12 µmMax
Particle Mesh Size 325 Mesh325 Mesh100% passing
pH 5.05.0
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Component Elements PropertiesMetricEnglishComments
Trace Metals <= 0.0010 %<= 0.0010 %Heavy Metals
 
Descriptive Properties
BaSO4 (%)98

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CIMBAR BariScan Ultra Chemically Purified White Barium Sulfate (BaSO4)
CIMBAR Miti-Wite B1 Chemically Purified White Barite (BaSO4)
CIMBAR BARA 200 Barium Sulfate (BaSO4)
CIMBAR Miti-Wite B3 Chemically Purified White Barite (BaSO4)
CIMBAR BARIMITE™ XF High Purity Barite (BaSO4)

CIMBAR916 / 133398

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.