MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Ketron™ CM GF30 Compression Molded, 30% Glass Reinforced Polyetherether Ketone
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Glass Fiber Filled

Material Notes: A compression molded, 30% glass fiber reinforced grade PEEK with excellent dimensional stability and outstanding chemical, corrosion, and creep resistance.

Vendors: TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.59 g/ccASTM D792
Water Absorption at Saturation 0.500 %ASTM D570 (17)
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1.00e+14 ohmANSI/ESD STM 11.11
Dielectric Strength 550 kV/inASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.0 µin/in-°FASTM E-831 (TMA)
Thermal Conductivity 2.98 BTU-in/hr-ft²-°F
Melting Point 644 °FASTM D3418
Maximum Service Temperature, Air 480 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 450 °FASTM D648
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Limited
Acids, Weak Acceptable
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Alkalies, Weak Acceptable
Chlorinated Solvents Acceptable
Continuous Sunlight Limited
Hot Water / Steam Acceptable
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Acceptable
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Ketron™ CM CA30 PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded
Overview of materials for Polyetheretherketone, Unreinforced
Mitsubishi Chemical Advanced Materials Ketron™ GF30 PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone
Mitsubishi Chemical Advanced Materials Ketron™ 1000 PEEK, Extruded Unfilled Polyetherether Ketone
Mitsubishi Chemical Advanced Materials Ketron™ CA30 PEEK, Extruded 30% Carbon Fiber Reinforced Polyetherether Ketone

P1SM17 / 20095

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.