MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Mitsubishi Chemical Advanced Materials Ketron® CA30 PEEK, Extruded 30% Carbon Fiber Reinforced Polyetherether Ketone
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: The addition of carbon fibers enhances the compressive strength and stiffness of PEEK, and dramatically lowers its expansion rate.

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.41 g/cc1.41 g/ccASTM D792
 1.41 g/cc1.41 g/ccASTM D792
Water Absorption 0.060 %0.060 %Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation 0.30 %0.30 %Immersion; ASTM D570(2)
 0.300 %0.300 %ASTM D570 (17)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 102102ASTM D785
 102102ASTM D785
Hardness, Shore D 90.090.0ISO 868
 9393ASTM D2240
Tensile Strength 131 MPa19000 psiASTM D638
 144 MPa20900 psiISO 527-1/-2 (7)
Tensile Strength at 150°C (300°F) 6.89 MPa1000 psiASTM D638
Tensile Strength at 65°C (150°F) 96.5 MPa14000 psiASTM D638
Elongation at Break 5.0 %5.0 %ASTM D638
Tensile Modulus 7.58 GPa1100 ksiASTM D638
Flexural Strength 177.5 MPa25750 psiASTM D790
 220 MPa31900 psiISO 178 (12)
Flexural Modulus 8.62 GPa1250 ksiASTM D790
Compressive Yield Strength  69.0 MPa
@Strain 1.00 %
10000 psi
@Strain 1.00 %
ISO 604 (10)
 125 MPa
@Strain 2.00 %
18100 psi
@Strain 2.00 %
ISO 604 (10)
 170 MPa
@Strain 5.00 %
24700 psi
@Strain 5.00 %
ISO 604 (10)
Compressive Strength 200 MPa29000 psi10% Def.; ASTM D695
Shear Strength 103 MPa14900 psiASTM D732
Izod Impact, Notched 0.550 J/cm1.03 ft-lb/inASTM D256 Type A
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.200.20Dry vs. Steel; QTM55007
K (wear) Factor 302 x 10-8 mm³/N-M150 x 10-10 in³-min/ft-lb-hrQTM 55010
Limiting Pressure Velocity 0.876 MPa-m/sec25000 psi-ft/min4:1 safety factor; QTM 55007
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square <= 1e+05<= 1e+05EOS/ESD S11.11
 1e+05 - 1.00e+7 ohm1e+05 - 1.00e+7 ohmANSI/ESD STM 11.11
Dielectric Strength 1.26 kV/mm32.0 kV/inShort Term; ASTM D149
 1.26 kV/mm32.0 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C10.0 µin/in-°FASTM E-831 (TMA)
 18.0 µm/m-°C
@Temperature -40.0 - 149 °C
10.0 µin/in-°F
@Temperature -40.0 - 300 °F
ASTM E831
 25.0 µm/m-°C
@Temperature 23.0 - 100 °C
13.9 µin/in-°F
@Temperature 73.4 - 212 °F
 25.0 µm/m-°C
@Temperature 23.0 - 150 °C
13.9 µin/in-°F
@Temperature 73.4 - 302 °F
 55.0 µm/m-°C
@Temperature >=150 °C
30.6 µin/in-°F
@Temperature >=302 °F
Thermal Conductivity 0.920 W/m-K6.38 BTU-in/hr-ft²-°F
 0.922 W/m-K6.40 BTU-in/hr-ft²-°F
 0.922 W/m-K6.40 BTU-in/hr-ft²-°FASTM F433
Melting Point 340 °C644 °FCrystalline, Peak; ASTM D3418
 340 °C644 °FASTM D3418
Maximum Service Temperature, Air 250 °C482 °FLong Term
 250 °C482 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 270 °C518 °FASTM D648
 270 °C518 °FASTM D648
Minimum Service Temperature, Air -20.0 °C-4.00 °F
Flammability, UL94 V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
Estimated Rating
 
Compliance PropertiesMetricEnglishComments
3A-Dairy NoNo
Canada AG NoNo
FDA NoNo
NSF NoNo
USDA NoNo
USP Class VI NoNo
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) LimitedLimited
 LimitedLimited
Acids, Weak AcceptableAcceptable
 AcceptableAcceptable
Alcohols AcceptableAcceptable
 AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
 AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
 AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
 AcceptableAcceptable
Conductive / Static Dissipative YesYes
Continuous Sunlight AcceptableAcceptable
 AcceptableAcceptable
Hot Water / Steam AcceptableAcceptable
 AcceptableAcceptable
Hydrocarbons - Aliphatic AcceptableAcceptable
 AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
 AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
 AcceptableAcceptable
Ketones, Esters AcceptableAcceptable
 AcceptableAcceptable
 
Descriptive Properties
ColorNatural
ESd categoryDissipative
Machinability71-10, 1=Easier to Machine

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Ketron® GF30 PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Ketron® CM CA30 PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Ketron® 1000 PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Data Sheet)
Overview of materials for Polyetheretherketone, Unreinforced
Mitsubishi Chemical Advanced Materials Ketron® LSG PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Datasheet)

P1SM17A / 20096

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.