MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polymer Resources PC-HM-FR2-[color]-4 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold Release  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 10% Glass Filled; Polycarbonate, Glass Fiber Filled, Flame Retardant

Material Notes: Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold Release

Process: Injection Molding
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.

Information provided by Polymer Resources Corporation.

Key Words: UL E113219
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.26 g/ccASTM D792
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cmASTM D955
Melt Flow 8.0 - 16 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 9500 psiASTM D638
Tensile Strength, Yield 8100 psiASTM D638
Flexural Strength 14900 psiASTM D790
Flexural Modulus 490 ksiASTM D790
Izod Impact, Notched 2.00 ft-lb/in
@Temperature 22.8 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 290 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 280 °FASTM D648
Flammability, UL94 V-0
@Thickness 1.50 mm
 V-0
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 560 - 600 °F
Middle Barrel Temperature 580 - 620 °F
Front Barrel Temperature 600 - 640 °F
Melt Temperature 575 - 625 °F
Mold Temperature 180 - 240 °F
Drying Temperature 245 - 255 °F
Dry Time 3.00 - 4.00 hour
Vent Depth 0.000500 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teijin Panlite® G-3410R Glass Fiber Reinforced Polycarbonate Resin
RTP Company RTP 80309 Polycarbonate, Long Glass Fiber 50%
RTP Company RTP 303 FR Polycarbonate (PC), Glass Fiber - Flame Retardant - Non-PBBO/E - UL94 V-0
PTS Tristar® PC-10GFR 10% Glass Reinforced Polycarbonate With Release
Covestro Makrolon® SF810 Polycarbonate, Glass Fiber Reinforced

PPOLYQ175 / 160695

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.