MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 80309 Polycarbonate, Long Glass Fiber 50%  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Glass Fiber Filled, Flame Retardant

Material Notes: Data is for injection molded specimens and was provided by the manufacturer, RTP Company.

This product has been discontinued, please contact RTP Company regarding alternate grades.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.63 g/cc0.0589 lb/in³ASTM D792
Water Absorption 0.070 %0.070 %24 hrs @ 23°C; ASTM D570
Linear Mold Shrinkage  0.0010 cm/cm
@Thickness 3.20 mm
0.0010 in/in
@Thickness 0.126 in
ASTM D955
 0.0020 cm/cm
@Thickness 6.35 mm
0.0020 in/in
@Thickness 0.250 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 119119ASTM D785
Tensile Strength, Ultimate 172 MPa24900 psiASTM D638
Elongation at Break 1.5 %1.5 %ASTM D638
Tensile Modulus 16.5 GPa2390 ksiASTM D638
Flexural Yield Strength 262 MPa38000 psiASTM D790
Flexural Modulus 12.4 GPa1800 ksiASTM D790
Izod Impact, Notched 2.70 J/cm
@Thickness 3.20 mm
5.06 ft-lb/in
@Thickness 0.126 in
ASTM D256
Izod Impact, Unnotched 10.7 J/cm
@Thickness 3.20 mm
20.0 ft-lb/in
@Thickness 0.126 in
ASTM D256
K (wear) Factor 10100 x 10-8 mm³/N-M5000 x 10-10 in³-min/ft-lb-hrat 50 fpm, 2000 PV against C1018 Steel HRC 15-25, 14-17 microsmoothness; ASTM D 3702
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Constant 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
Dry; ASTM D150
Dielectric Strength 17.0 kV/mm432 kV/inS/T; ASTM D149
Dissipation Factor 0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
Dry; ASTM D150
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 143 °C289 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 143 °C289 °FASTM D648
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
Values per RTP Company Testing; UL94

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celstran® PPS-GF40-01 PPS, 40% Glass Reinforced
Celanese Celstran® PPS-GF40-01 AD3002 Black PPS, 40% Glass Reinforced
LNP ULTEM® UCF1205 Polyetherimide, 12% Carbon Fiber Reinforcement, 5% PTFE Lubricant
Techmer ES HiFill® PPS GF40 BK 40% Glass Filled
RTP Company RTP 303 FR Polycarbonate (PC), Glass Fiber - Flame Retardant - Non-PBBO/E - UL94 V-0

PRRX96 / 66458

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.