MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Esenttia 16C12NA Impact Block Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Characteristics: Impact block copolymer polypropylene with good impact/stiffness balance and tough weld line.

Recommended for: Injection molding of rigid containers as pails, buckets, housewares and industrial applications.

Information provided by Esenttia by Propilco

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 16 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238B
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 21.72 MPa50 mm/min; ASTM D638
Elongation at Yield 6.5 %50 mm/min; ASTM D638
Flexural Modulus, 1% Secant 1103.2 MPa1.3 mm/min; ASTM D790-1A
Izod Impact, Notched 533.79 J/mASTM D256-A
Gardner Impact 31.64 JASTM D5420A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Esenttia 20C65NA Impact Block Copolymer Polypropylene
PolyMirae Moplen EP300L Injection Molding Grade Polypropylene
Borealis RB707CF Polypropylene Random Copolymer for Blown Film
LyondellBasell Alathon® M5372 High Density Polyethylene
ExxonMobil LDPE LD 157CW Blown Low Density Polyethylene Resin

PESEN049 / 184621

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.