MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik Kanthal APM Seamless tube and pipe
Categories: Metal; Superalloy; Iron Base

Material Notes: KANTHAL APM is an advanced powder metallurgical, dispersion strengthened, ferritic FeCrAl alloy which is used at tube temperatures up to 1250°C (2280°F). KANTHAL APM tubes have good form stability at high temperature. KANTHAL APM forms an excellent, non-scaling surface oxide, which gives good protection in most furnace environments, i.e. oxidizing, sulphurous and carbonaceous gas, as well as against deposits of carbon, ash, etc. The combination of excellent oxidation properties and formstability makes the alloy unique.

Typical applications for KANTHAL APM are as radiant tubes in electrically or gas fired furnaces such as continuous galvanizing furnaces, seal quench furnaces, holding furnaces and dosing furnaces in the aluminium, zinc, lead industries, thermocouple protection tubes, furnace muffles for sintering applications.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.10 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 225
Tensile Strength, Ultimate 687 MPa
Tensile Strength, Yield 475 MPa
Elongation at Break 11.3 %
Creep Strength 0.700 MPa
@Temperature 1200 °C
s-1: 1.0e­-10
 0.800 MPa
@Temperature 1200 °C
s-1: 1.0e­-8
 0.900 MPa
@Temperature 1100 °C
s-1: 1.0e­-10
 1.10 MPa
@Temperature 1100 °C
s-1: 1.0e­-8
 1.50 MPa
@Temperature 1000 °C
s-1: 1.0e­-10
 1.90 MPa
@Temperature 1200 °C
s-1: 1.0e­-6
 3.10 MPa
@Temperature 1100 °C
s-1: 1.0e­-6
 3.10 MPa
@Temperature 1000 °C
s-1: 1.0e­-8
 4.00 MPa
@Temperature 900 °C
s-1: 1.0e­-10
 6.00 MPa
@Temperature 1200 °C
s-1: 1.0e­-4
 6.70 MPa
@Temperature 1000 °C
s-1: 1.0e­-6
 6.80 MPa
@Temperature 900 °C
s-1: 1.0e­-8
 11.0 MPa
@Temperature 900 °C
s-1: 1.0e­-6
 11.0 MPa
@Temperature 1100 °C
s-1: 1.0e­-4
 13.0 MPa
@Temperature 1000 °C
s-1: 1.0e­-4
 20.0 MPa
@Temperature 900 °C
s-1: 1.0e­-4
 0.300 MPa
@Temperature 1200 °C,
Time 3.60e+6 sec
1% elongation
 0.700 MPa
@Temperature 1100 °C,
Time 3.60e+6 sec
1% elongation
 2.00 MPa
@Temperature 1000 °C,
Time 3.60e+6 sec
1% elongation
 5.90 MPa
@Temperature 900 °C,
Time 3.60e+6 sec
1% elongation
Rupture Strength 0.500 MPa
@Temperature 1200 °C,
Time 3.60e+7 sec
 2.00 MPa
@Temperature 1200 °C,
Time 360000 sec
 4.50 MPa
@Temperature 900 °C,
Time 3.60e+7 sec
 10.0 MPa
@Temperature 900 °C,
Time 360000 sec
Modulus of Elasticity 220 GPa
 130 GPa
@Temperature 1000 °C
 150 GPa
@Temperature 800 °C
 170 GPa
@Temperature 600 °C
 190 GPa
@Temperature 400 °C
 205 GPa
@Temperature 200 °C
 210 GPa
@Temperature 100 °C
Poissons Ratio 0.30
Shear Modulus 85.0 GPacalculated
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000145 ohm-cm
 0.000145 ohm-cm
@Temperature 100 °C
 0.000145 ohm-cm
@Temperature 200 °C
 0.000145 ohm-cm
@Temperature 300 °C
 0.000145 ohm-cm
@Temperature 400 °C
 0.000146 ohm-cm
@Temperature 500 °C
 0.000148 ohm-cm
@Temperature 600 °C
 0.000148 ohm-cm
@Temperature 700 °C
 0.000149 ohm-cm
@Temperature 800 °C
 0.000149 ohm-cm
@Temperature 900 °C
 0.000150 ohm-cm
@Temperature 1000 °C
 0.000150 ohm-cm
@Temperature 1100 °C
 0.000150 ohm-cm
@Temperature 1200 °C
 0.000150 ohm-cm
@Temperature 1300 °C
 0.000152 ohm-cm
@Temperature 1400 °C
Curie Temperature 600 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.0 µm/m-°C
@Temperature 20.0 - 250 °C
 12.0 µm/m-°C
@Temperature 20.0 - 500 °C
 14.0 µm/m-°C
@Temperature 20.0 - 750 °C
 15.0 µm/m-°C
@Temperature 20.0 - 1000 °C
 16.0 µm/m-°C
@Temperature 20.0 - 1200 °C
 16.0 µm/m-°C
@Temperature 20.0 - 1400 °C
Specific Heat Capacity 0.460 J/g-°C
@Temperature 20.0 °C
 0.560 J/g-°C
@Temperature 200 °C
 0.630 J/g-°C
@Temperature 400 °C
 0.710 J/g-°C
@Temperature 800 °C
 0.720 J/g-°C
@Temperature 1000 °C
 0.740 J/g-°C
@Temperature 1200 °C
 0.750 J/g-°C
@Temperature 600 °C
 0.800 J/g-°C
@Temperature 1400 °C
Thermal Conductivity 11.0 W/m-K
@Temperature 50.0 °C
 20.0 W/m-K
@Temperature 600 °C
 22.0 W/m-K
@Temperature 800 °C
 26.0 W/m-K
@Temperature 1000 °C
 27.0 W/m-K
@Temperature 1200 °C
 35.0 W/m-K
@Temperature 1400 °C
Melting Point 1500 °C
Maximum Service Temperature, Air 1250 °C
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.70fully oxidized
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 5.8 %
Carbon, C <= 0.080 %
Chromium, Cr 20.5 - 23.5 %
Iron, Fe >= 69.52 %
Manganese, Mn <= 0.40 %
Silicon, Si <= 0.70 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sandvik Kanthal APMT Seamless tube and pipe
AISI 1026 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
Aperam Resistohm® 125 Resistant Alloys Iron-Chromium-Aluminium Alloys
Goodfellow Aluchrom O® Resistance Alloy
Resistalloy International Fecralloy™ 135 Electrical Resistance Steel

NSANDV092 / 18986

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.