MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aperam Resistohm® 125 Resistant Alloys Iron-Chromium-Aluminium Alloys
Categories: Metal; Ferrous Metal

Material Notes: Resistohm 125 is a ferritic alloy of the FeCrAl family, which can be used at temperatures up to 1200°C. Resistohm 125 is particularly recommended for heating elements operating out in the open, in tubes quartz, in the emergent heaters, in the rheostats and in general where the temperature on the element is under 1100°C. Although it has a higher resistivity of 20 % than NiCr alloys, Resistohm 125 presents some inconveniences compared with Nickel-Chromium: Lower elongation at high temperature and More important fluctuation.

Information provided by Aperam

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.35 g/cc0.266 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 210210
Tensile Strength 700 MPa102000 psi
Tensile Strength, Yield 500 MPa72500 psi
Elongation at Break >= 18 %>= 18 %on 100 mm
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.000125 ohm-cm0.000125 ohm-cmTemperature coefficient = 0.00011/°C from 20 - 100°C
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.0 µm/m-°C
@Temperature 20.0 - 1000 °C
7.78 µin/in-°F
@Temperature 68.0 - 1830 °F
Thermal Conductivity 16.7 W/m-K
@Temperature 120 °C
116 BTU-in/hr-ft²-°F
@Temperature 248 °F
Melting Point 1520 °C2770 °F
Maximum Service Temperature, Air 1100 °C2010 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 3.0 %3.0 %
Chromium, Cr 17 %17 %
Iron, Fe 80 %80 %
 
Descriptive Properties
Creeping point1at 1000°C
 4at 800°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aperam Resistohm® 135 Resistant Alloys Iron-Chromium-Aluminium Alloys
AISI 1018 Steel, cold drawn
Aperam Resistohm® 145 Resistant Alloys Iron-Chromium-Aluminium Alloys
AISI 1006 Steel, cold drawn
AISI 1005 Steel

NPERA086 / 194875

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.