Natural color. E6046 exhibits high rigidity and mechanical strength. It is suitable for wide range of applications. Property data measured at room temperature, 50% RH. Information provided by Bieglo Gmbh for Ngai Hing Engineering Plastic (Hong Kong) Ltd. |