MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

NHEP Spectron™ E6046 Nylon 6, 15% Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: Natural color. E6046 exhibits high rigidity and mechanical strength. It is suitable for wide range of applications.

Property data measured at room temperature, 50% RH.

Information provided by Bieglo Gmbh for Ngai Hing Engineering Plastic (Hong Kong) Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ASTM D792
Linear Mold Shrinkage 0.0070 - 0.016 cm/cm0.0070 - 0.016 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 100 MPa14500 psiASTM D638
Elongation at Yield 8.0 %8.0 %ASTM D638
Flexural Strength 150 MPa21800 psiASTM D790
Flexural Modulus 4.30 GPa624 ksiASTM D790
Izod Impact, Notched 1.00 J/cm1.87 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 220 - 230 °C428 - 446 °F
Middle Barrel Temperature 230 - 240 °C446 - 464 °F
Front Barrel Temperature 240 - 250 °C464 - 482 °F
Nozzle Temperature 250 - 260 °C482 - 500 °F
Drying Temperature 100 - 120 °C
@Time 7200 - 14400 sec
212 - 248 °F
@Time 2.00 - 4.00 hour
 
Descriptive Properties
Processing Injection PressureMedium-High
Processing Injection SpeedMedium-High

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNGAI910 / 150496

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.