JS-B40G is an electrically conductive ink designed to produce circuits on non-porous substrates including ITO-coated substrates, PET, polyimide, and glass. JS-B40G ink is specially formulated for compatibility and stability with Dimatix printheads. A printing waveform for Dimatix DMP heads is available. |