MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil LD 12015.BA Low Density Polyethylene Resin (European Grade)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Product Description: ExxonMobil™ LD 12015.BA is an LDPE extrusion coating grade especially designed for coating on non-woven substrates. Its high melt-index combined with low density gives this grade the right balance between adhesion onto non-wovens, flexibility after coating and acts as a barrier for fluids and gases. ExxonMobil™ LD 12015.BA can also be used as a general extrusion and co-extrusion coating grade that requires easy processability, good neck-in/draw down balance and excellent heat sealability

Availability: Africa & Middle East and Europe

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: No
Applications:
  • Coextrusion Coating
  • Demanding Heat Seals
  • Document Plastification
  • Extrusion Coating
  • Extrusion Lamination
  • Food packaging
  • High Speed, Thin Weight Coatings
  • Industrial Packaging
  • Non-woven coating
  • Photographic Paper
  • Thermal Lamination

Information provided by ExxonMobil

Key Words: LDPE LD 259
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.915 g/ccExxonMobil method
Melt Flow 12 g/10 min190°C/2.16kg; ASTM D1238
Neck In 1.70 in
@Temperature 315 °C
656 ft/min, Constant output at 35 rpm; ExxonMobil Method
 1.80 in
@Temperature 315 °C
328 ft/min, Constant output at 35 rpm; ExxonMobil Method
Drawdown 9.17 m/s
@Temperature 315 °C
Constant output at 35 rpm; ExxonMobil Method
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 219 °FPeak Melting Point; ExxonMobil method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil LD 9519.LN Low Density Polyethylene Resin
ExxonMobil LD 8016.BA Low Density Polyethylene Resin (European Grade)
ExxonMobil LD 12015.48 Low Density Polyethylene Resin
Eastman 1390P Polyethylene

PEX99279 / 175515

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.