MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Tra-Con Tra-Duct 826D01 High Temperature Thermally Conductive Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: TRA-BOND 826D01 is a one part, high temperature conductive adhesive designed for die and heat sink attach in the automotive, aerospace, computer and optoelectronic assembly market. TRA-BOND 826D01 when fully cured exhibits superior adhesion to ceramics, glass, most metals, many plastics and other electronic materials. TRA-BOND 826D01 develops strong, durable electrically insulating/thermal conducting bonds with good impact properties, which are also resistant to galvanic action, weathering, water, salts, mild alkalis and acids, many petroleum products, and many other organic and inorganic compounds. This adhesive complies with the requirements of NASA`s Outgassing Specification when tested according to ASTM E-595-90.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 152000 cP
@Temperature 25.0 °C
152000 cP
@Temperature 77.0 °F
Mixed (sp #7, 10 rpm)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080
Adhesive Bond Strength 11.4 MPa1650 psiLap shear, alum to alum
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 55.0 °C131 °FUltimate Tg
 
Processing PropertiesMetricEnglishComments
Cure Time 30.0 min
@Temperature 100 °C
0.500 hour
@Temperature 212 °F
Pot Life 300 min300 min
 
Descriptive Properties
Color Light Tan
Outgassing, NASA, %CVCM0.0430 min @ 100°C
Outgassing, NASA, %TWL0.5230 min @ 100°C
Thixotropic Index 3.41 rpm/10 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTRAC167 / 71095

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.