MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman F-Cat HC Polyester Concentrate  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Applications:
  • Carpet Fibers

Product Description: Eastman Polymer F-Cat HC is a polyester concentrate intended to impart cationic dyeable properties to extruded polyester fibers. The primary application is a polyester BCF yarns intended for griege goods dyeing. The addition of Eastman Polymer F-Cat HC to extruded yarn supports interest in producing a multi-tonal carpet, that can be griege goods dyed to greatly differing colors when a finished carpet is produced from both traditional and cationic infused yarns. By varying the levels of concentration of Eastman Polymer F-Cat HC in the yarns, it would also be possible to produce different degrees of cationic colored goods.

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 51.6 lb/ft³
Viscosity Test 26 - 32 cm³/gInherent; EMN-A-AC-G-V-1
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 45.0 - 48.0 °CDry Polymer
 
Descriptive Properties
ColorPale Amber
FormPellets

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman AP005 Copolyester
Eastman Eastar CN015 Copolyester, High Flow Grade with Mold Release
Eastman Eastar CN005 Copolyester, High Flow Grade
Eastman AP006 Copolyester

PE8816 / 129661

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.