MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman Eastar CN015 Copolyester, High Flow Grade with Mold Release
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Applications:
  • Compacts
  • Cosmetic jar caps
  • Cosmetic jars
  • Cosmetics/personal care packaging
  • Fragrance caps
  • Fragrance packaging
  • Lip gloss containers
  • Lipstick containers
  • Personal care bottles

Key Attributes:

  • Ability to mold thick parts
  • Ease of processing
  • Easy to extrude, cut, decorate and seal
  • Excellent chemical resistance
  • Excellent clarity and color
  • Excellent colorability
  • Good impact strength
  • Good stiffness
  • High gloss appearance
  • Improved gate aesthetics
  • Readily fill intricate molds
  • Toughness

Product Description: Eastar CN015 copolyester is a high flow product that contains a mold release. It is the first copolyester resin from Eastman that has been designed and engineered specifically for cosmetics packaging applications. With its good color and clarity and ability to mold thick parts with improved gate aesthetics, Eastar CN is clearly the most suited copolyester for premium cosmetics packaging. Other features of Eastar CN are excellent chemical resistance, high gloss, and improvements in processing such as faster drying times, faster cycle times, and lower scrap rates. Eastar CN is also ideally suited for two-shot molding techniques due to its lower processing temperatures, very slow crystallization rate, and flow characteristics. This product has been GREENGUARD INDOOR AIR QUALITY CERTIFIED®.

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105105ASTM D785
Tensile Strength at Break 35.0 MPa5080 psiASTM D638
Tensile Strength, Yield 50.0 MPa7250 psiASTM D638
Elongation at Break 193 %193 %ASTM D638
Elongation at Yield 4.5 %4.5 %ASTM D638
Flexural Strength 67.0 MPa9720 psiASTM D790
Flexural Modulus 1.80 GPa261 ksiASTM D790
Izod Impact, Notched  0.380 J/cm
@Temperature -40.0 °C
0.712 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 0.700 J/cm
@Temperature 23.0 °C
1.31 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D4812
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ASTM D4812
Puncture Energy 40.0 J29.5 ft-lbAt Max load; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 71.0 °C160 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C145 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Haze <= 0.60 %<= 0.60 %ASTM D1003
Transmission, Visible 90 %90 %Total; ASTM D1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 205 - 240 °C401 - 464 °F
Mold Temperature 16.0 - 50.0 °C60.8 - 122 °F
Drying Temperature 50.0 °C122 °F
Dry Time 2 - 4 hour2 - 4 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman DuraStar DS2000 Polymer, Natural
Eastman DuraStar DS1000 Polymer, Natural
Eastman AP005 Copolyester
Eastman F-Cat HC Polyester Concentrate
Eastman Eastar DN011 Copolyester

PE8805 / 129650

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.