MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Indorama AlphaPet Preformance® 1708CC(A) PET Resin
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Description: Preformance® PET 1708CC(A) is a food grade PET copolymer that is used for various types of custom containers, including beverage and juice containers. It offers exceptional clarity and color. The low acetaldehyde content in the resin helps eliminate any impact on aroma and flavor. Preformance® PET 1708CC(A) resin is considered safe for food packaging applications based upon compliance with FDA Regulation 21 CFR Section 177.1630 specifications.

Key Words: Exceptional clarity and color
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.817 - 0.881 g/ccQCL-03-0004
Viscosity Test 78 - 82 cm³/gIntrinsic; QCL-03-0015
 
Chemical PropertiesOriginal ValueComments
Acetaldehyde <= 2.00 ppmQCL-03-0001
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.25 %as packed, QCK-03-0011
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
Color, CIE> 78 (L)QCL-03-0009
 -4.0 to 1.0 (b)QCL-03-0009
Contaminants/Black SpecsNoneQCL-03-0028
Dust<300 ppmas packed, QCL-03-0014
ProcessBlow Molding
 Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Indorama AlphaPet Preformance® 1708HS(A) PET Resin
Intercontinental Polymers HoPET 728-02 Clear, Polyester Pellets
Iran Petrochemical (PCC) PET BG-821 Polyethylene Terephthalate
Hippe PET Polyethylene Terephthalate
Iran Petrochemical (PCC) PET BG-800 Polyethylene Terephthalate

PINDOA901 / 126375

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.