MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
UNS C96200, Copper Casting Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal and Sand.

Applications: Components of items, being used for sea water corrosion resistance.

Classified under: Copper-nickels

Properties for as-sand-cast separately cast test bars (M01 temper). Alloy does not respond to heat treating

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.94 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate >= 310 MPa
Tensile Strength, Yield >= 172 MPa
Elongation at Break >= 20 %
Modulus of Elasticity 124 GPa
Compressive Strength 255 MPaat 0.1 mm/mm set
Fatigue Strength 13000 psi
@# of Cycles 1.00e+8
Reverse bend testing, as cast
Machinability 10 %UNS C36000 (free-cutting brass) = 100%
Charpy Impact 135 JV-notch
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000015674 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.376 J/g-°C
Thermal Conductivity 45.0 W/m-K
@Temperature 20.0 °C
Melting Point 1100 - 1150 °C
Solidus 1100 °C
Liquidus 1150 °C
Shrinkage 1.6 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.15 %
Copper, Cu 84.5 - 87 %
Iron, Fe 1.0 - 1.8 %
Lead, Pb <= 0.030 %
Manganese, Mn <= 1.5 %
Nickel, Ni 9.0 - 11 %
Niobium, Nb (Columbium, Cb) <= 1.0 %
Silicon, Si <= 0.30 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
UNS C96400, Copper Casting Alloy
UNS C96700, Copper Casting Alloy
Alpha Nickel-Aluminum Bronze, UNS C95800, Copper Casting Alloy
Copper nickel 10%, UNS C70600
Copper Nickel Tin UNS C96800, Copper Casting Alloy

MC96200b1 / 11969

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.