MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper Nickel Tin UNS C96800, Copper Casting Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes: This spinodal alloy is similar to the more common C96200, with higher strength. Common applications include pumps and fluid handling components for fresh or salt water.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.94 g/cc0.323 lb/in³(C96200)
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate >= 862 MPa>= 125000 psiAs Cast
 >= 931 MPa>= 135000 psiHeat Treated
Tensile Strength, Yield >= 689 MPa>= 100000 psiAs Cast
 >= 827 MPa>= 120000 psiHeat Treated
Elongation at Break 3.0 %3.0 %As Cast
Tensile Modulus 124 GPa18000 ksi(C96200)
Machinability 20 %20 %Based on Free cutting brass = 100%
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000156 ohm-cm0.0000156 ohm-cm(C96200)
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.1 µm/m-°C
@Temperature 20.0 - 300 °C
9.50 µin/in-°F
@Temperature 68.0 - 572 °F
C96200
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F(C96200)
Thermal Conductivity 29.4 W/m-K204 BTU-in/hr-ft²-°F(C96200)
Melting Point 1100 - 1150 °C2010 - 2100 °F(C96200)
Solidus 1100 °C2010 °F(C96200)
Liquidus 1150 °C2100 °F(C96200)
 
Processing PropertiesMetricEnglishComments
Precipitation Temperature 349 °C
@Time 299 sec
660 °F
@Time 0.0830 hour
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 78.72 - 82.9 %78.72 - 82.9 %As Remainder
Magnesium, Mg 0.0050 - 0.15 %0.0050 - 0.15 %
Manganese, Mn 0.050 - 0.30 %0.050 - 0.30 %
Nickel, Ni 9.5 - 10.5 %9.5 - 10.5 %
Niobium, Nb (Columbium, Cb) 0.10 - 0.30 %0.10 - 0.30 %
Tin, Sn 7.5 - 8.5 %7.5 - 8.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
UNS C96700, Copper Casting Alloy
Alpha Nickel-Aluminum Bronze, UNS C95800, Copper Casting Alloy
Aluminum Bronze, UNS C95500 Casting Alloy, TQ50 Temper
Copper Nickel Tin, UNS C72800
UNS C96200, Copper Casting Alloy

MC96800b1 / 11973

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.