MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro DUREFLEX® PT9200 TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Characterization: The Dureflex PT9200 series is a family of aromatic polyether polyurethane film/sheet products.

Properties / Applications: Dureflex PT9200 exhibits excellent hydrolysis and fungus resistance, and therefore are recommended for applications that have continuous exposure to water and high humidity environments. These products are recommended for adhesion to fabrics as a protective and adhesive layer, or as “stand alone ” films in demanding elastic applications. If your application will experience continuous exposure to petrochemicals such as gasoline, diesel fuel, aviation fuel, and many solvents, consider using Dureflex brand polyester polyurethane film and sheet grades. As with any product, use of Dureflex PT9200 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85ASTM D2240
Tensile Strength, Ultimate 9300 psiMD/CD Ave; ASTM D882
Elongation at Yield 625 %Ultimate; ASTM D882
100% Modulus 0.00758 GPa
@Strain 100 %
MD/CD Ave; ASTM D882
300% Modulus 0.0152 GPa
@Strain 300 %
MD/CD Ave; ASTM D882
Tear Strength 500 pliMD/CD Ave; ASTM D1004
 
Thermal PropertiesOriginal ValueComments
Softening Point 148 - 168 °CASTM E2347-004

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro DUREFLEX® PT6400 TPU
Covestro DUREFLEX® PS8400 TPU
Covestro DUREFLEX® PS8000 TPU
Covestro DUREFLEX® PS7000 TPU
Covestro DUREFLEX® PS5400 TPU

PCOVEST0768 / 202551

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.