MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Industeel Superplast® 350 Mold Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Tool Steel; Mold Steel

Material Notes: SUPERPLAST® 350 offers improved machinability, improved consistency and weldability, improved thermal conductivity, with a higher hardness allowing better mechanical properties and polishability. Improved mould life and reduction of maintenance costs lead to a higher productivity for moulders and end-users.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 340340
Tensile Strength, Ultimate 1130 MPa164000 psi
Tensile Strength, Yield 970 MPa141000 psi
Charpy Impact 15.0 J11.1 ft-lb
 40.0 J
@Temperature 100 °C
29.5 ft-lb
@Temperature 212 °F
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 38.0 W/m-K264 BTU-in/hr-ft²-°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for AISI 8000 Series Steel
AISI 8750 Steel (UNS G87500)
CeramTec 433 Alumina, 99.9%
International Mold Steel NAK-HH Precipitation Hardened Mold Steel
Materion ToughMet® 3 AT90 (OD≥4")

NINDUST72 / 17605

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.