MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

International Mold Steel NAK-HH Precipitation Hardened Mold Steel  (discontinued **)
Categories: Metal; Ferrous Metal; Tool Steel; Mold Steel

Material Notes: Description: NAK-HH is a precipitation, or age hardened mold steel with a through hardness of approximately 45/48 HRC. NAK-HH is ideal for use in plastic, composite and rubber molds where impact resistance is not critical. It is vacuum-arc re-melted steel with uniform grain structure, uniform hardness and excellent dimensional stability.

Unique Characteristics:

  • Vacuum-arc re-melt manufacturing process.
  • 45 HRC hardness.
  • Uniform hardness throughout, even in heavy sections.
  • Uniform grain structure with no pinholes, inclusions or hard spots.
  • Machines up to 30% faster than 30 HRC P20 mold steels.
  • Never needs stress relieving, even after heavy machining.

Information provided by International Mold Steel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 4545
Tensile Strength, Ultimate 1359 MPa197100 psiTransverse
 1385 MPa200900 psiLongitudinal
Tensile Strength, Yield  1009 MPa
@Strain 0.2 %
146300 psi
@Strain 0.2 %
Transverse
 1031 MPa
@Strain 0.2 %
149500 psi
@Strain 0.2 %
Longitudinal
Elongation at Break 4.0 %4.0 %Transverse
 11 %11 %Longitudinal
Reduction of Area 6.0 %6.0 %Transverse
 22 %22 %Longitudinal
Charpy Impact, Notched 11.0 J/cm²52.4 ft-lb/in²U-notch, Transverse
 16.0 J/cm²76.1 ft-lb/in²U-notch, Longitudinal

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Industeel Superplast® SP300 Prehardened Mold Steel
AISI Type O7 Tool Steel
International Mold Steel NAK55 Precipitation Hardened Mold Steel
AISI Type W1 Tool Steel, water quenched at 775°C (1425°F), tempered 350°C (660°F)
Industeel Superplast® 350 Mold Steel

NIMS02 / 17381

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.