MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Lupolen 4532D High Density Polyethylene, Steel Pipe Coating Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: Lupolen 4532D is a natural color, high-density polyethylene generally used in extrusion of steel pipe coating. It is primarily used as a top layer in conjunction with approved adhesives and fusion bonded epoxy (FBE) products to form a 3-layer corrosion protective coating system on steel pipelines with an operating temperature up to 85°C. With a bimodal molecular weight distribution and an improved thermal ageing resistance, Lupolen 4532D is designed for the stringent processing and performance requirements of steel pipe coating. Lupolen 4532D can be applied at high coating line speeds with a consistent coating thickness. Lupolen 4532D offers high resistance to impact, indentation, environmental stress cracking, chemicals, fungi and bacteria. Lupolen 4532D is available in natural, pellet form. It is not intended for food contact, medical or pharmaceutical applications.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density >= 0.500 g/ccASTM D1895
Density 0.949 g/ccASTM D1505
ESCR 100% Igepal® >= 1000 hourASTM D1693
Oxidative Induction Time (OIT) >= 20 min
@Temperature 220 °C
ASTM D3895
 >= 80 min
@Temperature 200 °C
ASTM D3895
Melt Flow 0.30 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 63ASTM D2240
Tensile Strength, Yield 3500 psi2"/min; ASTM D638
Elongation at Break >= 600 %ASTM D638
Tensile Modulus 147300 psi0.5"/min; ASTM D638
 
Thermal PropertiesOriginal ValueComments
Melting Point 129 °FASTM D3418
Vicat Softening Point 124 °CASTM D1525
Brittleness Temperature <= -76.0 °CASTM D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Lupolen 4261 A HDPE, Blow Molding Grade
Borealis Borcoat™ HE3453 Natural High Density Polyethylene for Steel Pipe Coating
Borealis Borcoat™ HE3450 Black High Density Polyethylene Top Coat for Steel Pipe Coating
Total XSene® 4206 B High Density Polyethylene - Steel Pipe Coating
LyondellBasell Lupolen 5261 Z Q 456 B High Density Polyethylene, Pipe and Sheet Extrusion Grade

PEQU0803 / 104159

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.