MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Deutsche Titan Tikrutan LT 27 Low-Alloyed Titanium  (discontinued **)
Categories: Metal; Nonferrous Metal; Titanium Alloy

Material Notes: Tikrutan LT 27 is a titanium alloy containing around 0.8% nickel and 0.3% molybdenum. LT 27 has better corrosion resistance than the commercially pure titanium grades but does not reach the corrosion resistance of the palladium-alloyed grades. When strength properties at room and elevated temperatures are required, however, LT 27 is superior to the materials RT 12 Pd and RT 15 Pd.

Information provided by Deutsche Titan

TiNiMo 083; DIN 3.7105; ASTM Grade 12

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.50 g/cc0.163 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 170170HB 30
Tensile Strength, Ultimate >= 480 MPa>= 69600 psi
Tensile Strength, Yield  >= 345 MPa
@Strain 0.2 %
>= 50000 psi
@Strain 0.2 %
 >= 370 MPa
@Strain 1 %
>= 53700 psi
@Strain 1 %
Elongation at Break >= 16 %>= 16 %Transverse; Bar and Stock Forgings
 >= 18 %>= 18 %Longitudinal; Bar and Stock Forgings
Reduction of Area >= 25 %>= 25 %
Modulus of Elasticity 103 GPa14900 ksi
 80.0 GPa
@Temperature 400 °C
11600 ksi
@Temperature 752 °F
Poissons Ratio 0.320.32calculated
Shear Modulus 39.0 GPa
@Temperature 20.0 °C
5660 ksi
@Temperature 68.0 °F
Izod Impact >= 27.0 J>= 19.9 ft-lbTransverse
 >= 34.0 J>= 25.1 ft-lbLongitudinal
Bend Radius, Minimum 4.0 t4.0 tAt Sheet s = 1
 8.0 t8.0 tAt Sheet s = 2
 20 t20 tAt Sheet s = 4
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000520 ohm-cm
@Temperature 20.0 °C
0.0000520 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  9.30 µm/m-°C
@Temperature 20.0 - 400 °C
5.17 µin/in-°F
@Temperature 68.0 - 752 °F
 9.50 µm/m-°C
@Temperature 20.0 - 200 °C
5.28 µin/in-°F
@Temperature 68.0 - 392 °F
Specific Heat Capacity  0.520 J/g-°C
@Temperature 20.0 °C
0.124 BTU/lb-°F
@Temperature 68.0 °F
 0.630 J/g-°C
@Temperature 400 °C
0.151 BTU/lb-°F
@Temperature 752 °F
Thermal Conductivity 19.0 W/m-K
@Temperature 20.0 °C
132 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 150 - 500 °C302 - 932 °FComplex; Hot Sheet Forming Temperature
 700 - 900 °C1290 - 1650 °FHot Forming Temperature
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.060 %<= 0.060 %
Hydrogen, H <= 0.013 %<= 0.013 %
Iron, Fe <= 0.25 %<= 0.25 %
Molybdenum, Mo 0.20 - 0.40 %0.20 - 0.40 %
Nickel, Ni 0.60 - 0.90 %0.60 - 0.90 %
Nitrogen, N <= 0.25 %<= 0.25 %
Oxygen, O <= 0.25 %<= 0.25 %
Titanium, Ti >= 97.877 %>= 97.877 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Platinum, Pt, CP Grade, Annealed
Titanium, Ti
Titanium Ti-5-5-8-3 (Ti-5Mo-5V-8Cr-3Al), 1 to 3 mm Sheet
Titanium Grade 12
Kobe Steel KSG12 Titanium alloy with low alloying elements, ASTM Gr. 12, Annealed

NDEUTI10 / 16106

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.