MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Petrothene® GA605034 Linear Low Density Polyethylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Applications
PETROTHENE GA 605 is a linear low density polyethylene designed for blown film applications requiring an enhanced combination of stiffness and strength. GA 605 can also be coextruded as a surface layer to enhance the clarity, gloss, printability and the heat seal of high molecular weight, high density polyethylene (HWW-HDPE) films. Applications include retail sacks, consumer can liners and packages, commercial and industrial packaging, as well as food packaging.

Processing Techniques
Recommended processing conditions for GA 605 are melt temperature of 400°- 450°F and a 1.5 - 3.0 blow-up ratio. Using proper techniques, this product can readily be drawn below 0.9 mil at optimum production rates. Specific recommendations for resin type and extrusion conditions can only be made when the end use, required properties and extrusion equipment are known.

Regulatory Status
GA 605 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food…" Specific limitations or conditions of use may apply.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³ASTM D1505
Thickness 25.4 microns1.00 mil2.5:1 BUR
Melt Flow 0.70 g/10 min0.70 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 550 %550 %ASTM D882
Film Elongation at Break, TD 625 %625 %ASTM D882
Dart Drop, Total Energy 1.49 J1.10 ft-lbASTM D4272
Elmendorf Tear Strength MD 150 g150 gASTM D1922
Elmendorf Tear Strength TD 700 g700 gASTM D1922
Dart Drop Test 150 g0.331 lbF50; ASTM D1709A
Film Tensile Strength at Break, MD 60.0 MPa8700 psiASTM D882
Film Tensile Strength at Break, TD 37.2 MPa5400 psiASTM D882
1% Secant Modulus, MD 338 MPa49000 psiASTM D882
1% Secant Modulus, TD 403 MPa58500 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 20 %20 %ASTM D1003
Gloss 40 %40 %45°; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
AntiblockHigh
Processing AidHigh
SlipHigh

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total Lumicene® mPE M5510 EP Metallocene Polyethylene, Blown Film
Total Lumicene® mPE M 4707 EP Metallocene Polyethylene, Blown Film
SABIC FI0644 Bimodal High Density Polyethylene for Blown Film
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade
LyondellBasell Petrothene® LR686001 High Density Polyethylene

PEQU0354 / 36797

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.