MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AK Steel Cold Rolled Carbon Steel, Extra Deep Drawing Steel Plus (EDDS+), Standard Grade
Categories: Metal; Ferrous Metal; Carbon Steel; Low Carbon Steel

Material Notes: Interstitial Free (I-F) steels are made by adding titanium and/or niobium to the molten steel after vacuum degassing and offer excellent drawability.

Information provided by AK Steel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.87 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 30
Tensile Strength, Ultimate 296 MPa
Tensile Strength, Yield 145 MPa
Elongation at Break 46 %in 2 inches
Modulus of Elasticity 200 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000142 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.9 µm/m-°C
@Temperature 20.0 - 100 °C
Specific Heat Capacity 0.481 J/g-°C
@Temperature 50.0 - 100 °C
Thermal Conductivity 93.0 W/m-K
 
Descriptive Properties
Deep-Drawing Capability rm1.9
Strain Hardening Exponent n0.25

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AK Steel Cold Rolled Carbon Steel, Extra Deep Drawing Steel (EDDS), Standard Grade
AK Steel Cold Rolled Carbon Steel, Drawing Steel (DS Type B), Standard Grade
SSAB Tunnplat Docol® DC05 (Fe P05) Deep-drawing Steel
Overview of materials for Epoxy, Cast, Unreinforced
Ti-25Al-10Nb-3V-1Mo Titanium Aluminide

NAKS032 / 14635

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.