MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M 7730FL Polyester Overlaminating Film
Categories: Polymer; Adhesive; Film

Material Notes: 3M™ Polyester Overlaminating Films utilize a clear or matte polyester film that is recommended for optimum durability and outdoor UV exposure. 3M™ Adhesive 400 offers excellent low temperature performance and long term aging for resistance to yellowing in outdoor applications.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 0.800 milAdhesive
 1.00 milFacestock
 1.50 milLiner
 
Mechanical PropertiesOriginal ValueComments
Peel Strength 1.50 pliStainless Steel, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
 1.50 pliPolyester, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
 2.125 pliPolyester, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 2.50 pliStainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 121 °C
Minimum Service Temperature, Air -40.0 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature >= -12.0 °CApplication
Shelf Life 24.0 Month
 
Descriptive Properties
Adhesive Type#400 Acrylic
LinerClear Polyester Liner

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyester Film
3M 856 General Purpose Polyester Tape
3M 850 Polyester Film Tape
3M 8422 Polyester Tape
3M 8421 Polyester Tape

PMM33448 / 168195

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.