MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M 8421 Polyester Tape
Categories: Polymer; Tape

Material Notes: 3M™ Polyester Tape 8421 is for photographic industry for splicing most film for processing through the developing chemicals.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 35.6 microns1.40 milBacking; ASTM D3752
 63.5 microns2.50 milTotal; ASTM D3752
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 125.6 MPa18220 psiASTM D3759
Elongation at Break 140 %140 %ASTM D3759
Peel Strength 0.5478 kN/m3.125 pliAdhesion to Steel; ASTM D3330
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 66.0 °C151 °F
 
Descriptive Properties
Adhesive TypeRubber with pigment
AppearanceCreamy white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M 8422 Polyester Tape
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Overview of materials for Polyester Film
3M 8992L Polyester Tape
3M 856 General Purpose Polyester Tape

PMM34492 / 169239

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.