MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Shandong Dongyue Shenzhou New Material Co Perfluoropropylenevinylether (PPVE)
Categories: Fluid

Material Notes: PPVE is a colorless transparent liquid and important monomer of organic fluoride material, which can also be used to introduce fluoride functional groups.

Main Applications:

PPVE is fluoride vinyl ether monomer to synthesize fluoride plastic. It can effectively destroy the crystallinity of TFE based copolymer. PPVE is widely used to synthesize fluoride polymer (PFA and modified PTFE, etc.) and fluoride functional groups can be introduced into organic molecules which are used in agriculture and pharmaceutical industry.

Information Provided by Shandong Dongyue Shenzhou New Material Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.53 g/cc
@Temperature 38.0 °C
Liquid
Molecular Weight 266.03 g/mol
Vapor Pressure 1.108 bar
@Temperature 37.8 °C
Saturated
 
Chemical PropertiesOriginal ValueComments
Critical Temperature 150.3 °C
 
Thermal PropertiesOriginal ValueComments
Boiling Point 35.0 °C
@Pressure 0.101 MPa
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not quantified
 
Descriptive Properties
CAS1623-05-8
Chemical NamePerfluoropropylenevinylether
Explosive Limit (%)1.1-47.0Volume
Molecular FormulaCF3CF2CF2OCFCF2
Purity (%)>97.51st Grade
 >99High Grade

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Methyl Ethyl Ketone (CH3CH2COCH3; 2-Butanone; MEK)
3M Novec™ 7000 Engineered Fluid
Hydrazoic Acid, HN3
Honeywell Dichloromethane
Furan (C4H4O)

PSHEN006 / 104061

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.