MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
North American Northern Red Oak Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Ring-Porous Hardwood. Data is based on small, clear, air-dried samples unless specified.
Usual surface texture: Medium
Dimensional changes when dried lumber is subjected to variations in humidity during service: Medium
Resistance to fungal decay (Heartwood in ground contact): Non-durable (5 to 10 years)
Resistance to penetration by preservatives: Moderately Resistant
Common Applications: Furniture. Interior joinery

Key Words: Quercus borealis; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.630 g/ccAir Dry (12-15% Moisture Content)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Wood Indentation 5700 NSide
Tensile Strength, Ultimate 5.50 MPaPerpendicular to Grain
Modulus of Rupture 0.0990 GPaStatic Bending
Flexural Modulus 12.56 GPaStatic Bending
Compressive Strength 8.60 MPaPerpendicular to Grain
 47.0 MPaParallel to Grain
Machinability 50 %Medium Relative to Other Wood
Shear Strength 12.3 MPaOrientation Unknown
Toughness 49.1 JTangential
 53.1 JRadial
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.00 BTU-in/hr-ft²-°FOven Dry
 1.20 BTU-in/hr-ft²-°F12% Moisture Content
Shrinkage 4.0 %Radial; Green to Zero Moisture
 8.2 %Tangential; Green to Zero Moisture
 13.5 %Volumetric; Green to Zero Moisture
 
Descriptive Properties
ColorYellowish-brown with red tingeUsual for heartwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
American Red Oak Wood
Laurel Red Oak Wood
European Red Oak Wood
Cherrybark Red Oak Wood
Black Red Oak Wood

PTSA130 / 71251

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.