MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Laurel Red Oak Wood
Categories: Wood and Natural Products; Wood; Hardwood

Key Words: Quercus Laurifolia; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.560 g/cc0.560 g/ccGreen, based on volume
 0.630 g/cc0.630 g/cc12% moisture content, based on volume
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 4448 N1000 lb (f)Green
 5382 N1210 lb (f)12% moisture content
Tensile Strength at Break 5.31 MPa770 psiGreen, perpendicular to grain
 5.45 MPa790 psi12% moisture content, perpendicular to grain
Modulus of Elasticity 9.58 GPa1390 ksiGreen
 11.7 GPa1690 ksi12% moisture content
Modulus of Rupture 0.0545 GPa7.90 ksiGreen
 0.0869 GPa12.6 ksi12% moisture content
Compressive Strength 3.93 MPa570 psiGreen, perpendicular to grain
 7.31 MPa1060 psi12% moisture content, perpendicular to grain
 21.9 MPa3170 psiGreen, parallel to grain
 48.1 MPa6980 psi12% moisture content, parallel to grain
Shear Strength 8.14 MPa1180 psiGreen, parallel to grain
 12.6 MPa1830 psi12% moisture content, parallel to grain
Impact 3939Impact bending in inches, 12% moisture content
 3939Impact bending in inches, green
Work to Maximum Load 0.0772 J/cm³11.2 in-lb/in³Green
 0.0814 J/cm³11.8 in-lb/in³12% moisture content
 
Thermal PropertiesMetricEnglishComments
Shrinkage 4.0 %4.0 %Radial, from green to oven dry, US origin
 9.9 %9.9 %Tangential, from green to oven dry, US origin
 19 %19 %Volumetric, from green to oven dry, US origin

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cherrybark Red Oak Wood
Pin Red Oak Wood
Scarlet Red Oak Wood
Water Red Oak Wood
Willow Red Oak Wood

PTSU032 / 71474

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.