MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Elite® 5100 Linear Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: ELITE® 5100 enhanced polyethylene resin is a copolymer produced via INSITE® Technology from Dow Plastics. It offers extremely high impact resistance, combined with excellent tear, tensile, and puncture properties for thick and thin gauge industrial and consumer blown film applications. ELITE 5100 resin exhibits a broader range and higher hot tack strengths than LLDPE, making it ideal for automated packaging applications. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2 (a) when used unmodified and processed according to good manufacturing practices.

Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.920 g/cc
Melt Flow 0.85 g/10 min
@Load 2.16 kg
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 11.4 MPa
Film Tensile Strength at Yield, TD 11.5 MPa
Film Elongation at Break, MD 645 %
Film Elongation at Break, TD 655 %
Secant Modulus, MD 0.200 GPaFilm value
Secant Modulus, TD 0.217 GPaFilm value
Elmendorf Tear Strength MD 907 gUnspecified film thickness
Elmendorf Tear Strength TD 1110 gUnspecified film thickness
Dart Drop Test >= 830 g
Film Tensile Strength at Break, MD 56.3 MPa
Film Tensile Strength at Break, TD 44.2 MPa
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 107 °C
 
Optical PropertiesOriginal ValueComments
Haze 11 %
 
Processing PropertiesOriginal ValueComments
Processing Temperature 101 °CSeal Initiation temperature
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Elite® 5110 Linear Low Density Polyethylene
Dow Elite® 5400 Linear Low Density Polyethylene
Dow DOWLEX™ 2025G Linear Low Density Polyethylene
Dow DOWLEX™ 2267A Linear Low Density Polyethylene, Blown Film Grade
SABIC 6821N Linear Low Density Polyethylene for Blown Film

PDW469 / 34538

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.