MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Elite® 5110 Linear Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: ELITE® 5110 enhanced polyethylene resin is a copolymer produced via INSITE® Technology from Dow Plastics. It offers unique combination of high modulus and excellent impact strength, allowing for downgauging in bag applications. In addition, ELITE 5110 resin has excellent tensile strength and good tear properties. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2 (a) when used unmodified and processed according to good manufacturing practices.

Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.926 g/cc0.0335 lb/in³
Melt Flow 0.85 g/10 min
@Load 2.16 kg
0.85 g/10 min
@Load 4.76 lb
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 14.0 MPa2030 psi
Film Tensile Strength at Yield, TD 15.0 MPa2180 psi
Film Elongation at Break, MD 615 %615 %
Film Elongation at Break, TD 640 %640 %
Secant Modulus, MD 0.228 GPa33.1 ksiFilm value
Secant Modulus, TD 0.2485 GPa36.04 ksiFilm value
Elmendorf Tear Strength MD 750 g750 gUnspecified film thickness
Elmendorf Tear Strength TD 1150 g1150 gUnspecified film thickness
Dart Drop Test 400 g0.882 lb
Film Tensile Strength at Break, MD 51.4 MPa7450 psi
Film Tensile Strength at Break, TD 44.5 MPa6450 psi
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 113 °C235 °F
 
Optical PropertiesMetricEnglishComments
Haze 13 %13 %
 
Processing PropertiesMetricEnglishComments
Processing Temperature 111 °C232 °FSeal Initiation temperature
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Elite® 5100 Linear Low Density Polyethylene
Dow ELITE™ 5401G Enhanced Polyethylene Resin
Dow DOWLEX™ 2025G Linear Low Density Polyethylene
Dow DOWLEX™ 2267A Linear Low Density Polyethylene, Blown Film Grade
SABIC 6821N Linear Low Density Polyethylene for Blown Film

PDW470 / 34539

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.