MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sika SikaFlex 219 LM Low Modulus Polyurethane Sealant
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: Sika 219 LM SikaFlex Low Modulus Polyurethane Sealant
This is a high performance, low modulus polyurethane base, non-sag elastomeric sealant with excellent adhesion to a wide variety of substrates. Meets Federal Specification TT-S-00230C, Type II, Class A and ASTM C-920, Type S, Grade NS, Class 25 and TT-S-001543A, Type non-sag. 12 - 15 mm Cut-Off. Excellent non-sag. Available in black, white, gray, tan, MB bronze, limestone. Cure Type: Moisture

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 10.3 lb/gal
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 15 - 25
Tensile Strength, Ultimate 125 psi
Elongation at Break >= 700 %
Adhesive Bond Strength 110 psi
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 170 °F
Minimum Service Temperature, Air -40.0 °F
 
Processing PropertiesOriginal ValueComments
Tack-Free Time 360 - 480 min
Shelf Life 12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Momentive Performance Materials RTV5222 White Adhesive Sealant, Low Modulus Paste
Sika SikaFlex® 255FC Fast Cure One Part Polyurethane Adhesive
Dymax 9001v3.0 Low Modulus Clear Microencapsulant
Epoxy Technology EPO-TEK® 310M-2 Optically Clear, Flexible Epoxy
Momentive Performance Materials RTV5223 Black Adhesive Sealant, Low Modulus Paste

PSIKA04 / 67722

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.