MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil LDPE LD 419.MV Low Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Product Description: LD 419.MV is a LDPE designed for wire and cable applications and is suitable for making crosslinkable compounds for medium voltage insulation.

Availability: Latin America, North America and South America

Applications:

  • Crosslinkable Compounds
  • Wire and Cable Compounds

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.921 g/ccExxonMobil method
Melt Flow 2.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 90
@Time 15.0 sec
ASTM D2240
Hardness, Shore D 44
@Time 15.0 sec
ASTM D2240
Tensile Strength at Break 1500 psiASTM D638
Tensile Strength, Yield 1700 psiASTM D638
Elongation at Break 630 %ASTM D638
Elongation at Yield 10 %ASTM D638
Flexural Modulus, 1% Secant 35000 psiASTM D790
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 7.60e+15 ohm-cmASTM D257
Dielectric Constant 2.3ASTM D150
Dielectric Strength 1300 V/milASTM D149
Dissipation Factor 0.000080ASTM D150
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 228 °FPeak Melting Point; ExxonMobil method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil LD 26019.LN Low Density Polyethylene Resin
ExxonMobil LD 40022.LI Low Density Polyethylene Resin
ExxonMobil LD 9519.LN Low Density Polyethylene Resin
Chevron Phillips Marlex® 1412 Injection Molding Resin
ExxonMobil LD 33021.07 Low Density Polyethylene Resin

PEX99232 / 175468

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.