MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Elektro-Isola G-Etronax SI Silicone, Glass Fabric Reinforcement, White, Sheets
Categories: Polymer; Thermoset; Silicone; Silicone, Molded, Glass Fiber Filled

Material Notes: Description: Electrical and electrotechnical applications. Suitable as high-frequency insulation on account of its dielectric loss. Used as, among other things, an insulation material in large induction furnaces for smelting metal. Can be used as material for lampshades in thicknesses under 0.4 mm on account of the material’s great flexibility, high heat resistance and color stability.

Information provided by Elektro-Isola

Key Words: IEC/EN 60893-3-1 SI GC 202, DIN 7735 Hgw 2572, NF C26 154 VS1&VS2, BS 3953 SI-4&5, NEMA LI 1 G-7
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.90 g/cc
@Temperature 23.0 °C
24h/23°C/50% RH; ISO 1183-A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 160 MPa
@Thickness >=1.50 mm
24h/23°C/50% RH; ISO 527
Flexural Strength 135 MPa
@Thickness >=1.50 mm,
Temperature 23.0 °C
24h/23°C/50% RH, Normal to laminate plane; ISO 178
Flexural Modulus 13.0 GPa
@Thickness >=1.50 mm
24h/23°C/50% RH, Normal to laminate plane; ISO 178
Compressive Strength 330 MPa
@Thickness >=5.00 mm
24h/23°C/50% RH, , Normal to laminate plane; ISO 604
Shear Strength 15.0 MPa
@Thickness >=5.00 mm
Parallel, 24h/23°C/50% RH; IEC 60893-2
Izod Impact, Notched (ISO) 45.0 kJ/m²
@Thickness >=5.00 mm
Parallel, 24h/23°C/50% RH; ISO 180/2A
 
Electrical PropertiesOriginal ValueComments
Insulation Resistance 1.00e+8 ohmafter immersion in water for 24 hr at 23°C; IEC 60167
Dielectric Constant 4.0
@Thickness <=3.00 mm,
Frequency 50 Hz
96h/105°C + 1h/23°C/20%RH; IEC 60250
 4.0
@Thickness <=3.00 mm,
Frequency 1e+6 Hz
96h/105°C + 1h/23°C/20%RH; IEC 60250
Dielectric Strength 7.00 kV/mm
@Thickness 3.00 mm,
Temperature 90.0 °C
after 1 hour in oil, Normal to laminate plane; IEC 60243-1
 50.0 kV/in
@Thickness >=3.00 mm,
Temperature 90.0 °C
after 1 hour in oil, Parallel to laminate plane; IEC 60243-1
Dissipation Factor 0.0030
@Thickness <=3.00 mm,
Frequency 50 Hz
96h/105°C + 1h/23°C/20%RH; IEC 60250
 0.0030
@Thickness <=3.00 mm,
Frequency 1e+6 Hz
96h/105°C + 1h/23°C/20%RH; IEC 60250
Comparative Tracking Index 400 V
@Thickness >=3.00 mm
24h/23°C/50% RH; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 210 °C
@Thickness >=3.00 mm,
Time 7.20e+7 sec
IEC 60216
Flammability Test 5.0
@Thickness 3.00 mm
IEC 60695-11-10
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Special Metals INCOLOY® Alloy 330
Sinotek Materials MD-4 Graphite Emulsion
Norplex-Micarta MC507U Silicone Glass Laminate Sheet, NEMA G-7
Elektro-Isola G-Etronax SI Silicone, Glass Fabric Reinforcement, White, Tubes
Carlson C 625 Nickel-Chromium-Molybdenum Alloy

PELEKT052 / 126928

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.