MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Elektro-Isola G-Etronax SI Silicone, Glass Fabric Reinforcement, White, Sheets
Categories: Polymer; Thermoset; Silicone; Silicone, Molded, Glass Fiber Filled

Material Notes: Description: Electrical and electrotechnical applications. Suitable as high-frequency insulation on account of its dielectric loss. Used as, among other things, an insulation material in large induction furnaces for smelting metal. Can be used as material for lampshades in thicknesses under 0.4 mm on account of the material’s great flexibility, high heat resistance and color stability.

Information provided by Elektro-Isola

Key Words: IEC/EN 60893-3-1 SI GC 202, DIN 7735 Hgw 2572, NF C26 154 VS1&VS2, BS 3953 SI-4&5, NEMA LI 1 G-7
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.90 g/cc
@Temperature 23.0 °C
0.0686 lb/in³
@Temperature 73.4 °F
24h/23°C/50% RH; ISO 1183-A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 160 MPa
@Thickness >=1.50 mm
23200 psi
@Thickness >=0.0591 in
24h/23°C/50% RH; ISO 527
Flexural Strength 135 MPa
@Thickness >=1.50 mm,
Temperature 23.0 °C
19600 psi
@Thickness >=0.0591 in,
Temperature 73.4 °F
24h/23°C/50% RH, Normal to laminate plane; ISO 178
Flexural Modulus 13.0 GPa
@Thickness >=1.50 mm
1890 ksi
@Thickness >=0.0591 in
24h/23°C/50% RH, Normal to laminate plane; ISO 178
Compressive Strength 330 MPa
@Thickness >=5.00 mm
47900 psi
@Thickness >=0.197 in
24h/23°C/50% RH, , Normal to laminate plane; ISO 604
Shear Strength 15.0 MPa
@Thickness >=5.00 mm
2180 psi
@Thickness >=0.197 in
Parallel, 24h/23°C/50% RH; IEC 60893-2
Izod Impact, Notched (ISO) 45.0 kJ/m²
@Thickness >=5.00 mm
21.4 ft-lb/in²
@Thickness >=0.197 in
Parallel, 24h/23°C/50% RH; ISO 180/2A
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance 1.00e+8 ohm1.00e+8 ohmafter immersion in water for 24 hr at 23°C; IEC 60167
Dielectric Constant  4.0
@Thickness <=3.00 mm,
Frequency 50 Hz
4.0
@Thickness <=0.118 in,
Frequency 50 Hz
96h/105°C + 1h/23°C/20%RH; IEC 60250
 4.0
@Thickness <=3.00 mm,
Frequency 1e+6 Hz
4.0
@Thickness <=0.118 in,
Frequency 1e+6 Hz
96h/105°C + 1h/23°C/20%RH; IEC 60250
Dielectric Strength  1.97 kV/mm
@Thickness >=3.00 mm,
Temperature 90.0 °C
50.0 kV/in
@Thickness >=0.118 in,
Temperature 194 °F
after 1 hour in oil, Parallel to laminate plane; IEC 60243-1
 7.00 kV/mm
@Thickness 3.00 mm,
Temperature 90.0 °C
178 kV/in
@Thickness 0.118 in,
Temperature 194 °F
after 1 hour in oil, Normal to laminate plane; IEC 60243-1
Dissipation Factor  0.0030
@Thickness <=3.00 mm,
Frequency 50 Hz
0.0030
@Thickness <=0.118 in,
Frequency 50 Hz
96h/105°C + 1h/23°C/20%RH; IEC 60250
 0.0030
@Thickness <=3.00 mm,
Frequency 1e+6 Hz
0.0030
@Thickness <=0.118 in,
Frequency 1e+6 Hz
96h/105°C + 1h/23°C/20%RH; IEC 60250
Comparative Tracking Index 400 V
@Thickness >=3.00 mm
400 V
@Thickness >=0.118 in
24h/23°C/50% RH; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 210 °C
@Thickness >=3.00 mm,
Time 7.20e+7 sec
410 °F
@Thickness >=0.118 in,
Time 20000 hour
IEC 60216
Flammability Test 5.0
@Thickness 3.00 mm
5.0
@Thickness 0.118 in
IEC 60695-11-10
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elektro-Isola G-Etronax SI Silicone, Glass Fabric Reinforcement, White, Tubes
Norplex-Micarta MC507U Silicone Glass Laminate Sheet, NEMA G-7
Carlson C 625 Nickel-Chromium-Molybdenum Alloy
ATI Allvac® 330 UNS N08330 Nickel Superalloy
Sinotek Materials MD-4 Graphite Emulsion

PELEKT052 / 126928

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.