MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AISI Type W1 Tool Steel, austenitized at 785-815°C (1450-1500°F)
Categories: Metal; Ferrous Metal; Carbon Steel; High Carbon Steel; Tool Steel; Water-Hardening Steel

Material Notes: The highest quality, water hardening carbon tool steel, controlled for hardenability and subject to the most rigid tests to ensure maximum uniformity in performance, with a composition held to closest limits.

Key Words: UNS T72301
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.83 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 575Converted from Rockwell C Hardness.
Hardness, Knoop 642Converted from Rockwell C Hardness.
Hardness, Rockwell C 56
Hardness, Vickers 619Converted from Rockwell C Hardness.
Tensile Strength, Ultimate 1475 MPa
Tensile Strength, Yield 1030 MPa
Elongation at Break 12 %in 50 mm
Modulus of Elasticity 205 GPa
Bulk Modulus 160 GPaTypical for steels.
Poissons Ratio 0.28
Machinability 40 %Based on AISI 1212 steel = 100%
Shear Modulus 80.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000300 ohm-cmat 20ºC
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.4 µm/m-°C
@Temperature 20.0 - 100 °C
 12.2 µm/m-°C
@Temperature 0.000 - 300 °C
 13.8 µm/m-°C
@Temperature 0.000 - 500 °C
Specific Heat Capacity 0.461 J/g-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity 48.0 W/m-K
 
Processing PropertiesOriginal ValueComments
Processing Temperature 175 - 345 °CTempering Temperature
 760 - 845 °CHardening Temperature
Annealing Temperature 740 - 790 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.70 - 1.5 %usually 0.90% to 1.10%
Chromium, Cr <= 0.15 %
Iron, Fe 97.2 - 99.2 %As Balance
Manganese, Mn 0.10 - 0.40 %
Molybdenum, Mo <= 0.10 %
Phosphorus, P <= 0.025 %
Silicon, Si 0.10 - 0.40 %
Sulfur, S <= 0.025 %
Tungsten, W <= 0.15 %
Vanadium, V <= 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type W1 Tool Steel, water quenched at 775°C (1425°F), tempered 350°C (660°F)
AISI Type W2 Tool Steel, water quenched at 775°C (1425°F), and tempered
AISI Type W2 Tool Steel, water quenched 775°C (1425°F), tempered 500°C (925°F)
Overview of materials for Water-Hardening Steel
AISI Type W5 Tool Steel

MSTW1C / 14108

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.