MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI Type W2 Tool Steel, water quenched 775°C (1425°F), tempered 500°C (925°F)
Categories: Metal; Ferrous Metal; Carbon Steel; High Carbon Steel; Tool Steel; Water-Hardening Steel

Key Words: UNS T72302
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.83 g/cc0.283 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1185 MPa171900 psi
Tensile Strength, Yield 1090 MPa158000 psi
Elongation at Break 11 %11 %
Modulus of Elasticity 205 GPa29700 ksi
Bulk Modulus 160 GPa23200 ksiTypical for steels.
Poissons Ratio 0.280.28Calculated
Machinability 40 %40 %Based on AISI 1212 steel = 100%
Shear Modulus 80.0 GPa11600 ksiTypical for steels.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000300 ohm-cm0.0000300 ohm-cmat 20ºC
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.4 µm/m-°C
@Temperature 20.0 - 100 °C
5.78 µin/in-°F
@Temperature 68.0 - 212 °F
 12.2 µm/m-°C
@Temperature 0.000 - 300 °C
6.78 µin/in-°F
@Temperature 32.0 - 572 °F
 13.8 µm/m-°C
@Temperature 0.000 - 500 °C
7.67 µin/in-°F
@Temperature 32.0 - 932 °F
Specific Heat Capacity 0.461 J/g-°C
@Temperature 0.000 - 100 °C
0.110 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity 48.0 W/m-K333 BTU-in/hr-ft²-°F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 175 - 345 °C347 - 653 °FTempering Temperature
 760 - 845 °C1400 - 1550 °FHardening Temperature
Annealing Temperature 740 - 790 °C1360 - 1450 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.60 - 1.4 %0.60 - 1.4 %usually 0.90% to 1.10%
Chromium, Cr <= 0.15 %<= 0.15 %
Iron, Fe 97.2 - 99.1 %97.2 - 99.1 %As Remainder
Manganese, Mn 0.10 - 0.40 %0.10 - 0.40 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si 0.10 - 0.40 %0.10 - 0.40 %
Sulfur, S <= 0.030 %<= 0.030 %
Vanadium, V 0.15 - 0.35 %0.15 - 0.35 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type W1 Tool Steel, water quenched at 775°C (1425°F), tempered 350°C (660°F)
AISI Type W1 Tool Steel, austenitized at 785-815°C (1450-1500°F)
AISI Type W2 Tool Steel, water quenched at 775°C (1425°F), and tempered
AISI Type W2 Tool Steel, water quenched 775°C (1425°F), tempered 700°C (1300°F)
AISI Type W5 Tool Steel

MSTW2B / 14110

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.