MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Baytec® AS Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Baytec AS is a elastomeric spray system for acoustics.

Properties / Applications: Baytec AS is a system for producing a solid, polyurethane elastomer which is processed on two component spray equipment and when filled with various mineral fillers (such as barium sulfate), can be used as the mass layer for NVH (Noise, Vibration and Harshness) applications. The Baytec AS system is a gray pigmented system. Fillers may be incorporated at levels as high as 80%. Baytec AS is a formulated PUR system supplied as two reactive liquid components. Component A is primarily a polymeric diphenylmethane diisocyanate (MDI). Component B is a blend of polyether polyols and additives. As with any product, use of Baytec AS system in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.850 g/cc0.850 g/ccASTM D792A
 1.04 g/cc1.04 g/ccPolyol
 1.24 g/cc1.24 g/ccIsocyanate
Viscosity 28 cP28 cPIsocyanate
 835 cP835 cPPolyol
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8585ASTM D2240
Tensile Strength, Ultimate 6.7138 MPa973.76 psiASTM D412, Die C
Elongation at Break 69 %69 %ASTM D412, Die C
Tear Strength 17.825 kN/m101.68 pliDie C; ASTM D412
 
Thermal PropertiesMetricEnglishComments
Flash Point 190 °C374 °FIsocyanate
 200 °C392 °FPolyol
 
Processing PropertiesMetricEnglishComments
Mold Temperature 60.0 - 71.0 °C140 - 160 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOVEST0233 / 202016

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.