MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond 813J01 Silicone Encapsulant
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: TRA-BOND 813J01 is a silicone adhesive system formulated to provide excellent thermal conductivity. This unique product bonds well to difficult substrates. Typical applications include encapsulation of heat generating devices such as transformers, thermistors or power sources and pour-in-place heat sinks. TRA-BOND 813J01 exhibits very low stress upon cure thus preventing component cracking and other stress related problems. It can be room temperature cured in thick or thin sections. This non-corrosive potting material will not revert when exposed to high temperatures. TRA-BOND 813J01 has a 6 month shelf life when stored at 25°C.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.10 g/ccMixed
Viscosity 40000 cPMixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75
Adhesive Bond Strength 500 psiLap shear, alum to alum
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 200 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 1.10 W/m-K
Maximum Service Temperature, Air 260 °C
Minimum Service Temperature, Air -65.0 °C
Glass Transition Temp, Tg -120 °CUltimate Tg
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 - 4.00 hour
@Temperature 65.0 °C
 20.0 min
@Temperature 150 °C
 48.0 - 168 hour
@Temperature 25.0 °C
Working Life 100 min100 grams
 
Descriptive Properties
Color Red
Mix Ratio, parts by weight100/100Resin/Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Semicosil® 970 TC A/B Conductive Adhesive Sealant
Tra-Con Tra-Duct 2919 Room Temperature Conductive, Flexible Silver Epoxy Adhesive
NuSil EPM-2493 Silicone, Thermal Interface Material (TIM): Adhesive
NuSil EPM-2490 Silicone, Thermal Interface Material (TIM): Adhesive
NuSil CV-2960 Silicone, Thermally Conductive

PTRAC158 / 71086

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.