MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Solvay DAPCO™ 3021C Low Viscosity, Self-Extinguishing Honeycomb Filler
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: DAPCO™ 3021C is a two-component, fast curing, low density, self-extinguishing epoxy honeycomb filler.

Features & Benefits:

  • Very low viscosity permits application by brush, spatula and trowel
  • Excellent adhesion to aluminum, Nomex® and balsa wood
  • Cures at low temperatures
  • Good chemical resistance, especially to aircraft fluids
  • 100% solids
Applications: DAPCO 3021C is commonly used for potting, stiffening and edge filling of honeycomb core. DAPCO 3011 is also used for aircraft interior repair.

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0300 g/cc
Solids Content 100 %Part A
 100 %Part B
 100 %Mixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 70
Elongation at Break 6.0 %
Flexural Modulus 300000 psi
Compressive Strength >= 1800 psi
 
Descriptive Properties
ColorWhitePart A
 WhitePart B
 YellowMixed
Mix Ratio2:1Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MarkeTech Silica Aerogel
Solvay DAPCO™ 3004 Rapid Cure Epoxy Adhesive & Repair Compound
Solvay DAPCO™ 3012 Self-Extinguishing, Low Density Honeycomb Filler
Solvay DAPCO™ 3050 Epoxy Potting Compound
Ultracor® UQF-95-1/4-3.0 Honeycomb Core Material

PCYTED018 / 180320

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.