MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ultracor® UQF-95-1/4-3.0 Honeycomb Core Material
Categories: Other Engineering Material; Composite Core Material

Material Notes: Construction: ±45° Quartz. Fiber: Astroquartz II. Ultracor® is a very low density honeycomb core material designed for use in highly weight-sensitive structures.  It is expected that it will be used in spacecraft Antenna Reflectors, Optical Benches, Solar Arrays, and other lightly loaded structures which must be positioned with accuracy and stability in order to properly perform their intended purpose. It was developed using a space qualified, toughened, polycyanate matrix resin. General Ultracor® features include low density, design flexibility, low CTE, low CME, and high thermal conductivity.

Data provided by Ultracor Inc., formerly YLA Cellular Products Company.

Key Words: Quartz Fiber Composite Core Material; Astroquartz II
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0480 g/cc0.00173 lb/in³core density
 
Mechanical PropertiesMetricEnglishComments
Compressive Yield Strength 1.55 MPa225 psi
Compressive Modulus 0.172 GPa24.9 ksi
Shear Modulus 0.117 GPa17.0 ksiribbon direction
Shear Strength 1.28 MPa186 psiribbon direction
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  1.042
@Frequency 9.50e+9 Hz
1.042
@Frequency 9.50e+9 Hz
Along ribbon
 1.06
@Frequency 9.50e+9 Hz
1.06
@Frequency 9.50e+9 Hz
Across ribbon
Dissipation Factor  0.00036
@Frequency 9.50e+9 Hz
0.00036
@Frequency 9.50e+9 Hz
Across ribbon
 0.00083
@Frequency 9.50e+9 Hz
0.00083
@Frequency 9.50e+9 Hz
Along ribbon

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ultracor® UCF-51-3/8-2.0 Honeycomb Core Material
Overview of materials for Epoxy, Molded, Glass Fiber Filler
Overview of materials for Melamine-Phenolic Copolymer
Ultracor® UKF-85-1/4-1.5 Honeycomb Core Material
MarkeTech Silica Aerogel

EYLA04 / 6141

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.