MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Coat 15C UV Curable Coating Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: TRA-COAT 15C is a clear, non-yellowing, UV curable nameplate coating that is ideal for applications that require a glossy, "lens-like" finish. TRA-COAT 15C will cure at a rate of 5-10 feet per minute with a 200 watt/inch medium pressure mercury vapor lamp. This photopolymer will also offer low shrinkage during cure and excellent stability thereafter. TRA-COAT 15C is a flexible material that offers excellent adhesion to many substrates including glass, most metals, and many plastics. TRA-COAT 15C has been used successfully in the lamination of nameplates, badges, labels, coating of plastic parts and also bonding applications in liquid crystal displays and other optical end products.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 1175 cP
@Temperature 25.0 °C
Mixed, ssa# 14, 100 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 83
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 11.0 °CUltimate Tg
 
Descriptive Properties
Color Clear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tra-Con Tra-Coat WCC2B UV Curable Optical Adhesive
Tra-Con Tra-Coat TC2 UV Cure Screen Printable Adhesive
Tra-Con Tra-Coat CF103B UV Curable Rigid Coating
Polynt ArmorFlex® ARMORFLEX 99F PA GEL COAT
Dow S 2260 PRIME COAT

PTRAC001 / 70929

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.