MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Tra-Con Tra-Coat CF103B UV Curable Rigid Coating
Categories: Other Engineering Material; Ceramic/Metallic Coating; Polymer; Adhesive; Thermoset

Material Notes: TRA-COAT CF103B is a high-gloss, UV curable polymer coating. It provides a wear layer with outstanding gloss retention, moisture resistance, stain resistance, and abrasion resistance. It can be used as a low maintenance finish for metals, plastics, and ceramics. It’s proven uses include ski and snowboard coating and decorative lamination. TRA-COAT CF103B will cure at 30 feet per minute at 300 watt/inch intensity.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity  130 cP
@Temperature 60.0 °C
130 cP
@Temperature 140 °F
Adhesive (cp #40, 20 rpm)
 215 cP
@Temperature 50.0 °C
215 cP
@Temperature 122 °F
Adhesive (cp #40, 20 rpm)
 350 cP
@Temperature 40.0 °C
350 cP
@Temperature 104 °F
Adhesive (cp #40, 20 rpm)
 670 cP
@Temperature 30.0 °C
670 cP
@Temperature 86.0 °F
Adhesive (cp #40, 20 rpm)
 1100 cP
@Temperature 25.0 °C
1100 cP
@Temperature 77.0 °F
Adhesive (cp #40, 20 rpm)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9595
Hardness, Shore D 6060
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 22.0 °C71.6 °FUltimate Tg
 
Descriptive Properties
Color ClearMixed/Cured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tra-Con Tra-Coat WCC2B UV Curable Optical Adhesive
Tra-Con Tra-Coat TC2 UV Cure Screen Printable Adhesive
Tra-Con Tra-Coat 15C UV Curable Coating Adhesive
Polynt ArmorFlex® ARMORFLEX 99F PA GEL COAT
Dow S 2260 PRIME COAT

PTRAC220 / 71148

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.