MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Akro-Plastic Akromid® A3 K1 FR black 950089 (2246) PA 6.6 Dry, 25% Glass Filled, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: AKROMID A3 K1 FR black 950089 (2246) is a 25% glass fiber reinforced, halogen-free flame retardant polyamide 6.6, all color listed at UL. Applications are switch housings in the electric industry.

Additive: Flame Retardant

Features:

  • Flame Retardant
  • Halogen Free
Uses:
  • Electrical/Electronic Applications
  • Housings
  • Switches

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.34 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0030 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.013 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 140 MPa5 [mm/min]; ISO 527-2
Elongation at Break 2.8 %5 [mm/min]; ISO 527-2
Tensile Modulus 9600 MPa1 [mm/min]; ISO 527-2
Flexural Strength 225 MPa2 [mm/min]; ISO 178
Flexural Modulus 9500 MPa2 [mm/min]; ISO 178
Flexural Strain at Break 3.0 %2 mm/min; ISO 178
Charpy Impact Unnotched >= 50.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 >= 50.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 9.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 10.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 550 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 262 °CDSC, 10K/min; DIN EN 11357-1
Flammability, UL94 V-0
@Thickness 0.800 mm
Oxygen Index 34 %ISO 4589-2
Glow Wire Ignition Temperature 750 °C
@Thickness 0.800 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 0.800 mm
IEC 60695-2-12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RheTech Products FRG130-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Flame Retardant, Black
Akro-Plastic Akromid® A3 K1 FR black 950089 (2246) PA 6.6 Conditioned, 25% Glass Filled, Flame Retardant
Avient Edgetek® AS-10GF/000 FR V0 BLACK Acrylonitrile Butadiene Styrene (ABS)
BASF Capron® 8232G HS FR 25% Glass-Filled Nylon 6 (Dry)
LATI Latene® AG3H2W G/30-V0 30% Glass Fiber with Chemical Bond, Heat-Stabilized Polypropylene Homopolymer (PPH)

PAKRO227 / 182814

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.