MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Capron® 8232G HS FR 25% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Fiber Filled, Flame Retardant

Material Notes: Capron 8232G HS FR is a 25% glass fiber reinforced, heat stabilized, flame retardant nylon 6 injection molding compound exhibiting excellent melt stability characteristics. It combines flame retardant ability with an excellent balance of high strength, stiffness and heat distortion temperature.

Capron 8232G HS FR is generally recommended for applications such as connectors, terminal blocks, switches and receptacles, coil bobbins, and appliance housings.

Data provided by Allied Signal.

Processing: Max. water content 0.16%. Product is supplied in sealed containers and drying is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 85°C (185 °F). Is recommended. Drying time is dependent on moisture level.

Melt Temperature: 250-280 degC (482-536 degF). Mold Temperature: 80-95 degC (176-203 degF). Injection and Packing Pressure: 35-125 bar (500-1500psi) This product can be processed over a wide range of mold temperatures; however, for applications where aesthetics critical, a mold surface temperature of 80-95 degC (176-203 degF) is required. Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off. Back pressure can be utilized to provide uniform melt consistency and reduce trapped air and gas. A maximum of 3.5 bar (50 psi) is recommended to minimize glass fiber breakage. Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing. Surface appearance is directly affected by injection rate.

Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.62 g/cc0.0585 lb/in³ISO data
Moisture Absorption at Equilibrium 1.1 %1.1 %50% RH; 23°C; ISO data
Water Absorption at Saturation 4.0 %4.0 %in water; 23°C; ISO data
Viscosity Measurement 5050Formic Acid Viscosity; ISO data
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inASTM Data MD
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 157 MPa22800 psiISO value at 5mm/min.
 160 MPa23200 psiASTM data at 5 mm/min.
Elongation at Break 3.0 %3.0 %ISO, 5 mm/min
 3.0 %3.0 %ASTM, 5 mm/min
Flexural Yield Strength 215 MPa31200 psiASTM Data
Flexural Modulus 8.965 GPa1300 ksiASTM Data
Poissons Ratio 0.350.35ISO data
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmISO data
Dielectric Strength 29.0 kV/mm737 kV/inISO data
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FASTM and ISO test
Deflection Temperature at 1.8 MPa (264 psi) 195 °C383 °FASTM Data
Flammability, UL94  V-0
@Thickness 0.840 mm
V-0
@Thickness 0.0331 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 5VA
@Thickness 2.50 mm
5VA
@Thickness 0.0984 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 275 °C527 °FSee Materials Notes
Mold Temperature 80.0 - 95.0 °C176 - 203 °F
 95.0 °C203 °FSee Materials Notes
Drying Temperature 85.0 °C185 °FSee Materials Notes
Injection Pressure 3.45 - 10.3 MPa500 - 1500 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LATI Latene® AG3H2W G/30-V0 30% Glass Fiber with Chemical Bond, Heat-Stabilized Polypropylene Homopolymer (PPH)
Akro-Plastic Akromid® A3 K1 FR black 950089 (2246) PA 6.6 Dry, 25% Glass Filled, Flame Retardant
BASF Ultramid® 8232G HS FR 25% Glass Fiber Fire Retardant PA6 (Conditioned)
BASF Capron® 8232G HS FR BK-102 25% Glass-Filled Nylon 6 (Dry)
RTP Company RTP 1805A FR  Polycarbonate/Acrylic Alloy (PC/PMMA) Glass Fiber 30% - Flame Retardant

PALC53 / 23847

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.