MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil HD 6510.17 Injection Molding Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: HD 6510 is a narrow molecular weight hexene copolymer designed for good processability and excellent balance of ESCR, Toughness, and Stiffness properties. This resin is ideally suited for a wide range of applications that require robust performance in conditions ranging from ambient to sub-zero temperatures.

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.945 g/cc0.0341 lb/in³ASTM D4883
Environmental Stress Crack Resistance 11 hour11 hourCond. B, 10%; ASTM D1693
Melt Flow 10 g/10 min10 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 21.39 MPa3103 psiat 500 mm; ASTM D638
Elongation at Break 69 %69 %at 500 mm; ASTM D638
Flexural Modulus, 1% Secant 704.6 MPa102200 psiASTM D790
Izod Impact, Notched 0.694 J/cm
@Temperature -40.0 °C
1.30 ft-lb/in
@Temperature -40.0 °F
ASTM D256
Tensile Impact Strength 208 kJ/m²
@Temperature -40.0 °C
99.2 ft-lb/in²
@Temperature -40.0 °F
ASTM D1822
 
Thermal PropertiesMetricEnglishComments
Melting Point 129 °C265 °FASTM D3418
Crystallization Temperature 113 °C235 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 58.7 °C138 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 37.6 °C99.7 °FASTM D648
Brittleness Temperature <= -70.0 °C<= -94.0 °FASTM D746
 
Descriptive Properties
FeaturesStandard Processing Antioxidants Stabilizer
FormPellet

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil HD 6510 Injection Molding Resin
Chevron Phillips Marlex® HMN 55180 High Density Polyethylene
Dow DOWLEX™ IP-41 High Density Polyethylene
ExxonMobil HD 6704.18 Injection Molding Resin
ExxonMobil HD 6733.17 Injection Molding Resin

PEXB062 / 37367

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.